An Experimental Study Of An Advanced Polymeric Material For Use In Total Knee Replacements Including Gait Analysis Of Mobile Knee Bearings, Lisa Ann Scott Oct 1996

An Experimental Study Of An Advanced Polymeric Material For Use In Total Knee Replacements Including Gait Analysis Of Mobile Knee Bearings, Lisa Ann Scott

Mechanical & Aerospace Engineering Theses & Dissertations

The primary objectives of this research were to clinically examine the New Jersey Low Contact Stress (LCS)™ Rotating Platform and Meniscal knee bearing systems and to investigate the tribological properties of a new polymer for potential application in total joint replacement. Thus, clinical studies were performed on subjects having the LCSTM Rotating Platform knee bearing and subjects having the LCS™ meniscal knee bearing. The results indicated that there was a statistically significant difference in the braking force for both implant groups when compared to a control group. There was also a statistically significant difference noted for the LCS™ Rotating Platform …


Study On Rheological Behavior Of The Composites Of Recycled Hdpe With Recycled Tire Rubber Particles, Yanze Li Jan 1996

Study On Rheological Behavior Of The Composites Of Recycled Hdpe With Recycled Tire Rubber Particles, Yanze Li

Masters Theses

This study was mainly concerned with rheological properties of composites of recycled high density polyethylene (HDPE) with recycled tire rubber particles at shear rates from 1.167 to 116.7 s-1. The viscosity was investigated in terms of effects of shear rate, shear stress, temperature, concentration of recycled tire rubber particles and heating duration. The temperature was in the range from 160 to 250 °C and the rubber particle concentration was between 0 and 25%. The heat duration for the composites was up to 240 minutes before testing.