Full-Text Articles in Materials Chemistry

Enhanced [Ru(Bpy)_3]~(2+)-Mediated Oxidation Of Guanine Prompted By Dhp, Bao-Lian Zhang, Wei Hong, Bao-Yi Lu, Hong Li Nov 2009

Enhanced [Ru(Bpy)_3]~(2+)-Mediated Oxidation Of Guanine Prompted By Dhp, Bao-Lian Zhang, Wei Hong, Bao-Yi Lu, Hong Li

Journal of Electrochemistry

The effects of dihexadecyl phosphate(DHP) and multi-walled carbon nanotubes(MWNTs) on the oxidation of guanine mediated by[Ru(bpy)3]2+ on the ITO electrode have been investigated by cyclic voltammetry and differential pulse voltammetry.The results showed that [Ru(bpy)3]2+ can mediate the oxidation.In the range from 0.01 to 0.15 mmol·L-1,peak currents for guanine oxidation mediated by [Ru(bpy)3]2+ increased with the rise of DHP concentrations.On the contrary,cationic surfactant HTAC has the ability to weaken the mediated oxidation of guanine.In addition,the oxidative mechanism of guanine mediated by [Ru(bpy)3]2+ with the participation of DHP is discussed.


Synthesis And Characterization Of Sulfur-Carbonnanotubes As Cathode Of Lithium/Sulfur Rechargeable Battery, Rui Du, Zhong-Zhi Yuan Aug 2009

Synthesis And Characterization Of Sulfur-Carbonnanotubes As Cathode Of Lithium/Sulfur Rechargeable Battery, Rui Du, Zhong-Zhi Yuan

Journal of Electrochemistry

A carbon-containing composite was synthesized by heating element sulfur and carbon nanotubes. The sulfur-carbonnanotube composites were characterized by X-ray diffraction,SEM,Brunauer-Emmett-Teller.The electrochemical property was characterized by cyclic voltammetry,constant current charge and discharge.It was revealed that the sulfur-carbonnanotube cathode 2016-type coin cells exhibited a good electrochemical property with the initial dicharge specific capacity up to 680 mAh/g and a stable capacity approximately 500 mAh/g after 30 cycle numbers.