Effect Of Dentin Biomodification Delivered By Experimental Acidic And Neutral Primers On Resin Adhesion, Lívia Tosi Trevelin, Yvette Alania, Mathew Mathew, Rasika S. Phansalkar, Shao-Nong Chen, Guido F. Pauli, Ana K. Bedran-Russo Aug 2020

Effect Of Dentin Biomodification Delivered By Experimental Acidic And Neutral Primers On Resin Adhesion, Lívia Tosi Trevelin, Yvette Alania, Mathew Mathew, Rasika S. Phansalkar, Shao-Nong Chen, Guido F. Pauli, Ana K. Bedran-Russo

School of Dentistry Faculty Research and Publications

Objectives

Proanthocyanidins (PACs) are biocompounds mimicking native collagen cross-links. The effective and practical delivery of any biocompound is pivotal for clinical usage. The aim was to investigate the dentin biomodification and effective formation of dentin–resin biointerfaces of two highly bioactive PAC-rich extracts, Vitis vinifera (Vv) and Camellia sinensis (Cs), delivered using neutral (NP) or acidic (AP) rinse-out primer approaches.

Methods

The depth of dentin demineralization (optical profilometry), dentin biomodification (apparent modulus of elasticity, collagen auto-fluorescence) and properties of dentin–resin interfaces (microtensile bond strength - μTBS, and micro-permeability) were investigated. NP consisted of either 15% Vv or Cs applied for …


Bond Strength Of An Amorphous Calcium Phosphate–Containing Orthodontic Adhesive, Jeff A. Foster, David W. Berzins, T. Gerard Bradley Mar 2008

Bond Strength Of An Amorphous Calcium Phosphate–Containing Orthodontic Adhesive, Jeff A. Foster, David W. Berzins, T. Gerard Bradley

School of Dentistry Faculty Research and Publications

Objective: To determine whether an amorphous calcium phosphate (ACP)-containing adhesive has an acceptable level of shear bond strength to be used as an orthodontic adhesive.

Materials and Methods: Sixty extracted premolars were randomly divided into three groups for orthodontic bonding. Group 1 used a composite resin adhesive (Transbond XT), group 2 was bonded with an ACP-containing adhesive (Aegis Ortho), and group 3 used a resin-modified glass ionomer (Fuji Ortho LC). All bonded teeth were stored in distilled water at 37°C for 40 ± 2 hours prior to debonding. Shear bond strength and adhesive remnant index (ARI) were recorded for each …


Shear Bond Strength Comparison Between Two Orthodontic Adhesives And Self-Ligating And Conventional Brackets, Rodney G. Northrup, David W. Berzins, T. Gerard Bradley, William I. Schuckit Jul 2007

Shear Bond Strength Comparison Between Two Orthodontic Adhesives And Self-Ligating And Conventional Brackets, Rodney G. Northrup, David W. Berzins, T. Gerard Bradley, William I. Schuckit

School of Dentistry Faculty Research and Publications

Objective: To evaluate and compare the shear bond strengths of two adhesives using two types of brackets: a conventional and a self-ligating bracket system.

Materials and Methods: Sixty extracted human premolars were collected. The premolars were randomly divided into three groups of 20 teeth. All three groups were direct bonded. Groups 1 and 2 used light-cured adhesive and primer (Transbond XT) with a conventional (Orthos) and a self-ligating bracket (Damon 2), respectively. Group 3 used a light-cured primer (Orthosolo) and a light-cured adhesive (Blūgloo) with a self-ligating bracket (Damon 2). The specimens were stored in distilled water at 37°C for …


A Comparison Of Bond Strength Between Direct- And Indirect-Bonding Methods, Brandon James Linn, David W. Berzins, Virendra B. Dhuru, T. Gerard Bradley Mar 2006

A Comparison Of Bond Strength Between Direct- And Indirect-Bonding Methods, Brandon James Linn, David W. Berzins, Virendra B. Dhuru, T. Gerard Bradley

School of Dentistry Faculty Research and Publications

The purpose of this study was to evaluate and compare the shear bond strength and the sites of bond failure for brackets bonded to teeth, using two indirect-bonding material protocols and a direct-bonding technique. Sixty extracted human premolars were collected and randomly divided into three groups. The direct-bonded group (group 1) used a light-cured adhesive and primer (Transbond XT). One indirect-bonded group (group 2) consisted of a chemical-cured primer (Sondhi Rapid Set) and light-cured adhesive (Transbond XT), whereas the other group (group 3) used a light-cured primer (Orthosolo) and adhesive (Enlight LV). Forty hours after bonding, the samples were debonded. …


Force To Debond Brackets From High-Fusing And Low-Fusing Porcelain Systems, Nicholas P. Ferri, Theodore Eliades, Spiros Zinelis, T. Gerard Bradley Mar 2006

Force To Debond Brackets From High-Fusing And Low-Fusing Porcelain Systems, Nicholas P. Ferri, Theodore Eliades, Spiros Zinelis, T. Gerard Bradley

School of Dentistry Faculty Research and Publications

The purpose of this study was to test the hypothesis that porcelain surface finishing, ie, low- and high-fusing porcelain, has an effect on the amount of force required to debond orthodontic brackets. A total of 20 high-fusing and 20 low-fusing porcelain specimens were prepared, polished, and bonded with standard edgewise brackets using a suggested porcelain bonding protocol. The brackets were debonded with a universal testing machine at shear mode. Resin removal was performed using two methods: a multifluted carbide bur with and without the use of Sof-Lex polishing discs. Representative specimens were studied under a scanning electron microscope before and …


Bond Strength Of Direct And Indirect Bonded Brackets After Thermocycling, Jacob Daub, David W. Berzins, Brandon James Linn, T. Gerard Bradley Mar 2006

Bond Strength Of Direct And Indirect Bonded Brackets After Thermocycling, Jacob Daub, David W. Berzins, Brandon James Linn, T. Gerard Bradley

School of Dentistry Faculty Research and Publications

Thermocycling simulates the temperature dynamics in the oral environment. With direct bonding, thermocycling reduces the bond strength of orthodontic adhesives to tooth structure. The purpose of this study was to evaluate the shear bond strengths (SBS) of one direct and two indirect bonding methods/adhesives after thermocycling. Sixty human premolars were divided into three groups. Teeth in group 1 were bonded directly with Transbond XT. Teeth in group 2 were indirect bonded with Transbond XT/Sondhi Rapid Set, which is chemically cured. Teeth in group 3 were indirect bonded with Enlight LV/Orthosolo and light cured. Each sample was thermocycled between 5°C and …