Bond Strength Of An Amorphous Calcium Phosphate–Containing Orthodontic Adhesive, Jeff A. Foster, David W. Berzins, T. Gerard Bradley Sep 2015

Bond Strength Of An Amorphous Calcium Phosphate–Containing Orthodontic Adhesive, Jeff A. Foster, David W. Berzins, T. Gerard Bradley

T. Gerard Bradley

Objective: To determine whether an amorphous calcium phosphate (ACP)-containing adhesive has an acceptable level of shear bond strength to be used as an orthodontic adhesive. Materials and Methods: Sixty extracted premolars were randomly divided into three groups for orthodontic bonding. Group 1 used a composite resin adhesive (Transbond XT), group 2 was bonded with an ACP-containing adhesive (Aegis Ortho), and group 3 used a resin-modified glass ionomer (Fuji Ortho LC). All bonded teeth were stored in distilled water at 37°C for 40 ± 2 hours prior to debonding. Shear bond strength and adhesive remnant index (ARI) were recorded for each …


Force To Debond Brackets From High-Fusing And Low-Fusing Porcelain Systems, Nicholas P. Ferri, Theodore Eliades, Spiros Zinelis, T. Gerard Bradley Sep 2015

Force To Debond Brackets From High-Fusing And Low-Fusing Porcelain Systems, Nicholas P. Ferri, Theodore Eliades, Spiros Zinelis, T. Gerard Bradley

T. Gerard Bradley

The purpose of this study was to test the hypothesis that porcelain surface finishing, ie, low- and high-fusing porcelain, has an effect on the amount of force required to debond orthodontic brackets. A total of 20 high-fusing and 20 low-fusing porcelain specimens were prepared, polished, and bonded with standard edgewise brackets using a suggested porcelain bonding protocol. The brackets were debonded with a universal testing machine at shear mode. Resin removal was performed using two methods: a multifluted carbide bur with and without the use of Sof-Lex polishing discs. Representative specimens were studied under a scanning electron microscope before and …


A Comparison Of Bond Strength Between Direct- And Indirect-Bonding Methods, Brandon James Linn, David W. Berzins, Virendra B. Dhuru, T. Gerard Bradley Sep 2015

A Comparison Of Bond Strength Between Direct- And Indirect-Bonding Methods, Brandon James Linn, David W. Berzins, Virendra B. Dhuru, T. Gerard Bradley

T. Gerard Bradley

The purpose of this study was to evaluate and compare the shear bond strength and the sites of bond failure for brackets bonded to teeth, using two indirect-bonding material protocols and a direct-bonding technique. Sixty extracted human premolars were collected and randomly divided into three groups. The direct-bonded group (group 1) used a light-cured adhesive and primer (Transbond XT). One indirect-bonded group (group 2) consisted of a chemical-cured primer (Sondhi Rapid Set) and light-cured adhesive (Transbond XT), whereas the other group (group 3) used a light-cured primer (Orthosolo) and adhesive (Enlight LV). Forty hours after bonding, the samples were debonded. …


Bond Strength Of Direct And Indirect Bonded Brackets After Thermocycling, Jacob Daub, David W. Berzins, Brandon James Linn, T. Gerard Bradley Sep 2015

Bond Strength Of Direct And Indirect Bonded Brackets After Thermocycling, Jacob Daub, David W. Berzins, Brandon James Linn, T. Gerard Bradley

T. Gerard Bradley

Thermocycling simulates the temperature dynamics in the oral environment. With direct bonding, thermocycling reduces the bond strength of orthodontic adhesives to tooth structure. The purpose of this study was to evaluate the shear bond strengths (SBS) of one direct and two indirect bonding methods/adhesives after thermocycling. Sixty human premolars were divided into three groups. Teeth in group 1 were bonded directly with Transbond XT. Teeth in group 2 were indirect bonded with Transbond XT/Sondhi Rapid Set, which is chemically cured. Teeth in group 3 were indirect bonded with Enlight LV/Orthosolo and light cured. Each sample was thermocycled between 5°C and …


Shear Bond Strength Comparison Between Two Orthodontic Adhesives And Self-Ligating And Conventional Brackets, Rodney G. Northrup, David W. Berzins, T. Gerard Bradley, William I. Schuckit Sep 2015

Shear Bond Strength Comparison Between Two Orthodontic Adhesives And Self-Ligating And Conventional Brackets, Rodney G. Northrup, David W. Berzins, T. Gerard Bradley, William I. Schuckit

T. Gerard Bradley

Objective: To evaluate and compare the shear bond strengths of two adhesives using two types of brackets: a conventional and a self-ligating bracket system. Materials and Methods: Sixty extracted human premolars were collected. The premolars were randomly divided into three groups of 20 teeth. All three groups were direct bonded. Groups 1 and 2 used light-cured adhesive and primer (Transbond XT) with a conventional (Orthos) and a self-ligating bracket (Damon 2), respectively. Group 3 used a light-cured primer (Orthosolo) and a light-cured adhesive (Blūgloo) with a self-ligating bracket (Damon 2). The specimens were stored in distilled water at 37°C for …


Microtensile Bond Strength Of Resin-Dentin Bonds Following Application Of A Chemical Collagen Cross-Linker Using Different Dentin Bonding Systems, Bassam Naoraldean Zidane Jul 2015

Microtensile Bond Strength Of Resin-Dentin Bonds Following Application Of A Chemical Collagen Cross-Linker Using Different Dentin Bonding Systems, Bassam Naoraldean Zidane

Student Theses, Dissertations and Capstones

Introduction: The stabilization of dentinal collagen fibers against enzymatic degradation by the use of biocompatible cross-linker agents is of clinical importance for effective dentin bonding to surpass the test of time.

Objective: The present study aims to evaluate and compare the effect of the application of two versions of a desensitizer solution to sound coronal dentin, on the microtensile bond strength (μTBS) of the resin-sound coronal dentin using 4th and 6th generation dentin bonding systems.

Materials and Methods: Extracted human third molars were collected from an unidentified bank of teeth followed by IRB approval. A flat surface of all 12 …


Effect Of Surface Preparation On The Shear Bond Strength Of Orthodontic Brackets Bonded To Zirconia : An In-Vitro Study, Nathaniel Wieder Jan 2015

Effect Of Surface Preparation On The Shear Bond Strength Of Orthodontic Brackets Bonded To Zirconia : An In-Vitro Study, Nathaniel Wieder

Student Theses, Dissertations and Capstones

Objectives: The purpose of this in-vitro study was to evaluate the effects of three different surface preparation methods on the shear bond strength of orthodontic brackets bonded to zirconia and determine the most appropriate method. Methods: 45 zirconia and 30 leucite-reinforced porcelain mandibular premolar crowns were divided into 5 groups and received the following surface preparations: 37% phosphoric acid and non-hydrolyzed silane, 4% hydrofluoric acid and hydrolyzed silane, microetch with 50μ Al 2 O3 particles. A universal adhesive primer containing MDP was applied and the brackets were bonded with a bis-GMA composite resin. Shear bond strength (SBS) at bond …