Effect Of Copper Addition On Mechanical Properties And Electrical Conductivity Of Pp/C-Cu Bipolar Plate Composites, Anne Zulfia, Taufik Abimanyu, Verina Warga Dalam Nov 2011

Effect Of Copper Addition On Mechanical Properties And Electrical Conductivity Of Pp/C-Cu Bipolar Plate Composites, Anne Zulfia, Taufik Abimanyu, Verina Warga Dalam

Makara Journal of Technology

Effect of Copper Addition on Mechanical Properties and Electrical Conductivity of PP/C-Cu Bipolar Plate Composites. Bipolar plate is a major component in PEM fuel cell which possess main function of collecting and removing electrons from anode to cathode. Therefore, materials for bipolar plates produced must have high electrical conductivity. To obtain bipolar plate materials which is cheap, lightweight and high conductivity, so it is developed bipolar plates material based on PP/C-Cu composite. PP/C-Cu composites has been made by mixing all materials then compounding, rheomix, hot blending and hot press. Cu (Copper) has been used various from 0.1 wt%, 1 wt% …


Medium Density Fibreboard Made Of Acetylated Sludge From Paper Mill, Luthfi Hakim, Evalina Herawati, I Nyoman Jaya Wistara Nov 2011

Medium Density Fibreboard Made Of Acetylated Sludge From Paper Mill, Luthfi Hakim, Evalina Herawati, I Nyoman Jaya Wistara

Makara Journal of Technology

Medium Density Fibreboard Made of Acetylated Sludge from Paper Mill. Research of using sludge as raw material for making medium density fibreboard (MDF) was useful to create additional value of sludge. The objective of the research was to evaluate physical properties, mechanical properties, and durability of MDF from acetylated sludge in 4 levels of acetate anhydride (0%, 3%, 5%, and 7%) with 3 replicates. The MDF was made using dry process. After materials were mixed with adhesives, they were pressed using hotpress under 170 oC temperature and 45 Pa pressure for 25 minutes. The size of the MDF sample was …