Wear Behavior Of Tini And Tini-Tic Clads Deposited By Tig Surfacing, Masoud Harooni, Morteza Shamanian, Alireza Fadaei Tehrani Jan 2012

Wear Behavior Of Tini And Tini-Tic Clads Deposited By Tig Surfacing, Masoud Harooni, Morteza Shamanian, Alireza Fadaei Tehrani

Masoud Harooni

This paper deals with the investigation of wear behavior of TiNi and TiNi-TiC clads applied to plain carbon steel by tungsten inert gas (TIG) surfacing process. In this regard, ball milled Ti-Ni and Ti-Ni-C powder mixtures were used as feedstock materials. The clad layers were investigated using X-ray diffractometery (XRD), scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), hardness measurements and reciprocating wear tests. The results of microhardness measurements indicated that hardness values of TiNi-TiC composites were higher than those of TiNi by approximately 100HV. It was also shown that the wear behavior of TiNi-TiC clads was better than that …


Mitigation Of Pore Generation In Laser Welding Of Magnesium Alloy Az31b In Lap Joint Configuration, Masoud Harooni, Fanrong Kong, Blair Carlson, Radovan Kovacevic Jan 2012

Mitigation Of Pore Generation In Laser Welding Of Magnesium Alloy Az31b In Lap Joint Configuration, Masoud Harooni, Fanrong Kong, Blair Carlson, Radovan Kovacevic

Masoud Harooni

Magnesium, as the lightest structural metal, has been widely used in the automotive and aerospace industries. Porosity is the main issue in the welding of magnesium alloys and can be caused by surface coatings, hydrogen gas, pre-existing porosity, the collapse of an unstable keyhole and vaporization of alloying elements. In this study, the effect of the oxide layer on pore generation in the welding of AZ31B-H24 magnesium alloy is investigated. A fiber laser with a power of up to 4 kW is used to weld samples in a lap joint configuration. Two groups of samples are studied: as received (AR) …


تعيين عرض تختال در ورودي كوره هاي پيش گرم ناحيه نورد گرم مجتمع فولاد مباركه با استفاده از پردازش ديجيتال تصاوير, Eaman Alibeigi, Rasoul Amirfattahi, Masoud Harooni, Hamid Montazerolghaem Nov 2008

تعيين عرض تختال در ورودي كوره هاي پيش گرم ناحيه نورد گرم مجتمع فولاد مباركه با استفاده از پردازش ديجيتال تصاوير, Eaman Alibeigi, Rasoul Amirfattahi, Masoud Harooni, Hamid Montazerolghaem

Masoud Harooni

هر يك از تختال هاي توليد شده در بخش ريخته گري مداوم ناحيه فولاد سازي، پس از مارك زني و تعيين مشتري به يكي از دو صورت هوايي يا سيالي خنك شده و در زمان مقرر به وسيله غلطك هايي وارد كوره پيش گرم مي شوند. در اين مرحله، 1/6 mm تختال تا حرارت 1100 درجه سانتيگراد گرم شده و عمليات نورد گرم بر روي آن به منظور تهيه ورق فولاد با ضخامت صورت مي گيرد. تعيين دقيق مشخصات ابعادي تختال ها از جمله طول، عرض و ضخامت آنها قبل از ورود به كوره هاي پيش گرم و تطبيق دادن …


Gtaw ايجادشده با روش جوشکاری Tini-Tic و Tini بررسی ريزساختاری پوشش, Masoud Harooni, Morteza Shamanian, Alireza Fadaei Tehrani Oct 2008

Gtaw ايجادشده با روش جوشکاری Tini-Tic و Tini بررسی ريزساختاری پوشش, Masoud Harooni, Morteza Shamanian, Alireza Fadaei Tehrani

Masoud Harooni

هدف از انجام اين پژوهش بهبود سختي سطحي و ريزساختار فولاد ساده کربنی از نوع 52 و مقايسه ريز ساختار اين دو با هم GTAW ايجاد شده به روش جوشکاری TiNi-TiC و TiNi پوششی از بترتيب با نسبت استوکيومتری مساوي و نسبت ۲۰ Ti-Ni-C و Ti-Ni است. بدين منظور مخلوط پودری به طور جداگانه توسط روش فعال سازی مکانيکی فعال شد و سپس بر سطح TiC درصد تقويت کننده به ضخامت ۱ ميليمتر پيش نشانده شده با استفاده از روش جوشکاری قوسی St نمونه های فولادی 52 تنگستن- گاز ذوب و با فلز پايه امتزاج يافته است. جهت بررسي نوع …