Full-Text Articles in Engineering

A Study And Simulation Of Flux Induced Corrosion In Copper Tubing Used For The Distribution Of Potable Water, Daniel O. Benham Jun 2019

A Study And Simulation Of Flux Induced Corrosion In Copper Tubing Used For The Distribution Of Potable Water, Daniel O. Benham

Materials Engineering

Water side corrosion within copper plumbing can occur due to a wide variety of unwanted circumstances. Through the controlled immersion of six ¾” copper tubing samples with five utilizing a unique industry standard soldering flux, this investigation associates residual flux deposits with the initiation of pitting in copper. Water stagnation in a copper potable water distribution system, typically associated with an infrequently used faucet, is a condition highly prone to copper pitting. A test apparatus designed to produce a partially stagnant flow condition with scheduled electrolyte flushes every 3 days was developed and constructed to contain 6 test samples for …


Effect Of Solder Joint Flux Residue On Medical Guide Wire Performance, Rebecca Lisberg, Enlly Bugarin Rodriguez Jun 2019

Effect Of Solder Joint Flux Residue On Medical Guide Wire Performance, Rebecca Lisberg, Enlly Bugarin Rodriguez

Materials Engineering

The effect of residual soldering flux on the mechanical properties of 304 stainless-steel core medical guide wires was analyzed. A soldering process joins the metallic components of the distal end of a medical guide wire product. Acidic soldering flux is used to prepare the surfaces of the metallic substrates. Manufacturing protocol utilizes an ultrasonic bath to remove excess flux from the soldered joints. Sample groups underwent different levels of cleaning: no cleaning, partial cleaning, and full ultrasonic bath cleaning to obtain varying residual flux levels. Experimental sample groups underwent corrosion acceleration in an environmental chamber at 37°C and 85% relative …