Behaviour Of New Zealand Ironsand During Iron Ore Sintering, Zhe Wang, Harold Rogers, David Pinson, Brian J. Monaghan, Sheng Chew, Paul Zulli, Sharon Nightingale, Guangqing Zhang Sep 2014

Behaviour Of New Zealand Ironsand During Iron Ore Sintering, Zhe Wang, Harold Rogers, David Pinson, Brian J. Monaghan, Sheng Chew, Paul Zulli, Sharon Nightingale, Guangqing Zhang

Brian Monaghan

Titanium-bearing burdens are commonly introduced into blast furnaces to protect the hearlh because the so-called "titanium bear" which is a precipitate of carbide, nitride and carbonitride of titanium may form in the blast furnace hearth if Ti02 is present in the feed [1 , 2J. New Zealand ironsand is a titanomagnetite, containing around 60 wt.% iron, 8 wt.% titanium and other substances such as silica, phosphorus and lime [3, 4]. Since it is competitive in price, introduction of the ironsand into the ferrous feed can reduce the production cost and potentially increase blast furnace campaign life. An appropriate method of …


Strength And Bonding In Reduced Ironsand-Coal Compacts, R J. Longbottom, B J. Monaghan, S A. Nightingale, J G. Mathieson Sep 2014

Strength And Bonding In Reduced Ironsand-Coal Compacts, R J. Longbottom, B J. Monaghan, S A. Nightingale, J G. Mathieson

Brian Monaghan

In this investigation, the strength and bonding within reduced ironsand-coal compacts were studied, with the aim of better understanding the binding mechanisms in the reduced compacts and, based on this understanding, to improve their strength. Ironsand ore and sub-bituminous coal were mixed and pressed into compacts, which were reduced by heating in a thermogravimetric furnace to temperatures between 1273 and 1573 K under argon. The progress of the reaction was monitored by measuring the weight loss with time. The reduced compacts were found to have low strength in compression testing. The main form of bonding between the reduced ironsand particles …