Synthesis Of Bisphenol A Bis-2-Hydroxypropylmethacrylate (Bisgma) And Diethylchlorophosphate And 2-Hydroxyethylmethacrylate (Decp-Hema) And Preparation Of Dental Adhesives, Da Xie
Theses
BisGMA and DECP-HEMA were separately synthesized from Bisphenol A and glycidyl methacrylate and from diethylchlorophosphate and 2-hydroxyethyl-methacrylate. The structure of the monomer, BisGMA, was further analyzed by means of chromatography, VPO, IR, FTIR and GC-MASS.
Based on the main monomers, BisGMA, DECP-HEMA and an organosilane compound, a dental adhesive has been formulated. Although the tervile strength of the adhesive has been found to be not as good as the adhesive formulated by a previous worker (student), its applicability to teeth is more suitable for clinic practice.
Preparation And Testing Of Novel Dental Adhesives Based On Bis- Gma/Tegdma Monomer System, Deyun Sun
Preparation And Testing Of Novel Dental Adhesives Based On Bis- Gma/Tegdma Monomer System, Deyun Sun
Theses
In this study, polymerizable phosphonate adhesives synthesized from Diethylchloro-phosphate and 2-Hydroxyethylmethylacrylate and formulated with G-methacryloxy-propyltrimethoxy silane is used in Bis-GMA/TEGDMA monomer system. All the raw materials and finished products are characterized with infrared spectra, vapor pressure osmometry, viscosity and gel test. The bonding strength to tooth materials is determined by Instron machine. The work emphasizes applying polymeric organic phosphonate adhesive to Bis-GMA/TEGDMA monomer system and investigates the appropriate conditions for the crosslinking of Bis-GMA/TEGDMA monomer system. Average bonding strength of 744 psi to enamel and 600 to dentine are ob¬tained in comparision to 550 psi to enamel for phosphonate/silane/MMA/PMMA and …