Thermal Stability Of Electrodeposited Liga Ni-W Alloys For High Temperature Mems Applications
Thermal Stability Of Electrodeposited Liga Ni-W Alloys For High Temperature Mems Applications
A.S. Md Abdul Haseeb
For thermally stable LIGA materials for high temperature MEMS applications LIGA Ni-W layers and micro testing samples with different compositions (15 and 5 at% W) were electrodeposited. In order to investigate the thermal stability the Ni-W layers were annealed at different temperatures (300-700°C) and for different durations (1, 4, 16 h). Their microstructure and micro-hardness were than analysed after annealing and compared with those of as-deposited states. The observed microstructures show, in comparison to pure LIGA nickel, a small grain growth and a relatively stable structure up to 700°C. The micro-hardness values of the LIGA Ni-W layers are higher than …
High-Throughput Screening Of Shape Memory Alloy Thin-Film Spreads Using Nanoindentation, Arpit Dwivedi, Thomas J. Wyrobek, Oden L. Warren, Jason R. Hattrick-Simpers, Olubenga O. Famodu, Ichiro Takeuchi
High-Throughput Screening Of Shape Memory Alloy Thin-Film Spreads Using Nanoindentation, Arpit Dwivedi, Thomas J. Wyrobek, Oden L. Warren, Jason R. Hattrick-Simpers, Olubenga O. Famodu, Ichiro Takeuchi
Faculty Publications
We have demonstrated the utility of nanoindentation as a rapid characterization tool for mapping shape memoryalloy compositions in combinatorial thin-film libraries. Nanoindentation was performed on Ni–Mn–Al ternary composition spreads. The indentation hardness and the reduced elastic modulus were mapped across a large fraction of the ternary phase diagram. The large shape memoryalloy composition region, located around the Heusler composition (Ni2MnAl), was found to display significant departure in these mechanical properties from the rest of the composition spread. In particular, the modulus and the hardness values are lower for the martensite region than those of the rest of the …