Open Access. Powered by Scholars. Published by Universities.®

Engineering Commons

Open Access. Powered by Scholars. Published by Universities.®

2020

CHEMISTRY AND CHEMICAL ENGINEERING

Catalysis and Reaction Engineering

Arrhenius equation

Articles 1 - 2 of 2

Full-Text Articles in Engineering

Research Of Kinetic Characteristics Of The Process Of Decomposition Of Zinc Concentrate With Hydrochloric Acid, Rosilov Mansur, Deng Tianlong, Usmanov Ilham, Samadiy Murodjon Oct 2020

Research Of Kinetic Characteristics Of The Process Of Decomposition Of Zinc Concentrate With Hydrochloric Acid, Rosilov Mansur, Deng Tianlong, Usmanov Ilham, Samadiy Murodjon

CHEMISTRY AND CHEMICAL ENGINEERING

The aim of the study was the theoretical justification of the kinetic characteristics of the process of producing zinc chloride from zinc concentrate of the Khandiza deposit. For this, the effect of temperature and duration of the process of autoclave zinc extraction in a 28% hydrochloric acid solution was studied at a ratio of Zn: HCI = 1:1.1. Variable parameters were the temperature of 70, 80 and 90 °C and the duration of the leaching process of 6, 8 and 10 hours. The optimal parameters for the production of zinc chloride were determined.


Research Of Kinetic Characteristics Of The Process Of Decomposition Of Zinc Concentrate With Hydrochloric Acid, Rosilov Mansur, Deng Tianlong, Usmanov Ilham, Samadiy Murodjon Jun 2020

Research Of Kinetic Characteristics Of The Process Of Decomposition Of Zinc Concentrate With Hydrochloric Acid, Rosilov Mansur, Deng Tianlong, Usmanov Ilham, Samadiy Murodjon

CHEMISTRY AND CHEMICAL ENGINEERING

The aim of the study was the theoretical justification of the kinetic characteristics of the process of producing zinc chloride from zinc concentrate of the Khandiza deposit. For this, the effect of temperature and duration of the process of autoclave zinc extraction in a 28% hydrochloric acid solution was studied at a ratio of Zn: HCI = 1:1.1. Variable parameters were the temperature of 70, 80 and 90 °C and the duration of the leaching process of 6, 8 and 10 hours. The optimal parameters for the production of zinc chloride were determined.