Full-Text Articles in Engineering

Effect Of Carbon On Primary Alpha Percentage In Ti-6al-4v As Temperature Approaches The Beta Transus, Kyle Savage Jun 2013

Effect Of Carbon On Primary Alpha Percentage In Ti-6al-4v As Temperature Approaches The Beta Transus, Kyle Savage

Materials Engineering

Some Ti-6Al-4V forgings require a specific amount of α phase known as primary α in the finished product. The percentage of primary α is dependent on how close to the beta transus temperature forging is conducted. The beta transus temperature is affected by certain alloying elements. Carbon is one of the elements known to increase the beta transus temperature. Since each Ti-6Al-4V ingot contains varying amounts of carbon, testing on a variety of chemistries needs to be conducted. Cubes approximately 0.5 inches from low, medium, and high carbon chemistries were heat treated at temperatures below the beta transus in 18 …


Evaluation Of Forging Strain For Maximum Grain Size In Open-Die Forged 6061 Aluminum, Eric Strehl Jun 2013

Evaluation Of Forging Strain For Maximum Grain Size In Open-Die Forged 6061 Aluminum, Eric Strehl

Materials Engineering

In an effort to maximize grain growth of open-die forged 6061 aluminum alloy parts, samples from three of Weber Metals’s suppliers (Hidal Co-Almex USA Inc., TST Inc., and Vista Metals Corp.; to be called Supplier H, Supplier T, Supplier V respectively) were cut into cylinders with diameters of 0.75˝ and heights of 2˝, and put through a simulated forging process and heat treatment. It is possible that additional alloying elements may be promoting or inhibiting grain growth in the final part. Maximizing grain growth for aluminum alloy parts results in improved resistance to intergranular corrosion. Samples from each vendor had …