Molecular Dynamics Study Of Creep Deformation In Nickel-Based Superalloy, Sabila Kader Pinky Jan 2019

Molecular Dynamics Study Of Creep Deformation In Nickel-Based Superalloy, Sabila Kader Pinky

MSU Graduate Theses

The present study employs molecular dynamics simulations of Ni-based superalloy to investigate the creep behavior under uniaxial compression test. Dislocation dynamics is analyzed for the nickel-based single crystal superalloy with the presence of void and with varying the distribution of gamma-prime phase The results show that multiple-void systems are more prone to yield than single-void systems and single-void systems are more prone to yield than the system without void. From the simulations, it has been determined that the creep mechanism in Ni/Ni3Al is subject to change on the applied stress depending on the distribution of gamma-prime phases change. Dislocation behavior …