Effect Of Ion Implantation On The Mechanical Properties Of The Grain And Grain Boundary Regions Of Inconel X750, Maisaa Nezar Tawfeeq Oct 2019

Effect Of Ion Implantation On The Mechanical Properties Of The Grain And Grain Boundary Regions Of Inconel X750, Maisaa Nezar Tawfeeq

Electronic Thesis and Dissertation Repository

Annulus gas spacers in CANada Deuterium Uranium (CANDU) nuclear reactors are made from the heat-treated Inconel X750 Nickel-based alloy. This alloy is designed to have high strength and creep resistance at elevated temperature. Unlike other reactor designs, the CANDU reactor has a high thermal neutron fluence, which results in an enhancement of the radiation damage and the internal production of helium and hydrogen. They are thus susceptible to microstructural instability and mechanical property degradation with time. Studies of ex-service spacers have indicated that they display intergranular embrittlement and lower ultimate tensile strength compared to nonirradiated Inconel X750. The primary degradation …