Fabrication And Magnetic Properties Of Fe Nanostructures In Anodic Alumina Membrane, J H. Lim, W S. Chae, H O. Lee, L Malkinski, S G. Min, J B. Wiley, J H. Jun, S H. Lee, J S. Jung Jan 2010

Fabrication And Magnetic Properties Of Fe Nanostructures In Anodic Alumina Membrane, J H. Lim, W S. Chae, H O. Lee, L Malkinski, S G. Min, J B. Wiley, J H. Jun, S H. Lee, J S. Jung

Physics Faculty Publications

Several Fe nanostructures with different lengths, diameters, and separations of the constituting magnetic components have been synthesized using anodized alumina membranes (AAMs) to understand the influence of these parameters on their magnetic properties. Fe nanostructures with high crystallinity and (110) orientation were synthesized by electrodeposition at room temperature in regular AAMs and mild-hard AAM (Mi-Ha AAM). Fe nanostructures with different aspect ratios (1:1, 1:10, and 1:75) in the form of nanodots, nanorods, or nanowires were synthesized in regular AAMs with the 100 nm interpore distance. Mi-Ha AAMs with two different pore sizes (70 and 120 nm) and 250 nm interpore …


Morphology, Magnetic And Dynamic Properties Of Artificial Structures Assembled By Acoustic Vibrations, K B. Paul, L Malkinski Jan 2009

Morphology, Magnetic And Dynamic Properties Of Artificial Structures Assembled By Acoustic Vibrations, K B. Paul, L Malkinski

Physics Faculty Publications

Cobalt micromagnetic particles with an average size of ≈ 1.6 μm and varying total mass of the powder were assembled on patterned media with perpendicular magnetization by acoustic vibrations onto designed shapes reflecting the primary material. The replicas were studied with scanning electron microscopy, vibrating sample magnetometry, and ferromagnetic resonance spectroscopy. Their properties were significantly influenced by the shape anisotropy induced through the parent molds. A tendency in the development of the physical characteristics of the replicas was observed as their geometrical parameters changed.


The Temperature Dependence Of Hysteretic Processes In Co Nanowires Arrays, I Astefanoaei, I Dumitru, A Diaconu, L Spinu, A Stancu Jan 2008

The Temperature Dependence Of Hysteretic Processes In Co Nanowires Arrays, I Astefanoaei, I Dumitru, A Diaconu, L Spinu, A Stancu

Physics Faculty Publications

In this paper, the temperature dependence of the hysteretic processes of Co nanowires, squarelly ordered in an array prepared by electrodeposition in nanopores of alumina membranes was analyzed. Both the magnetostatic interactions induced in the nanowires arrays and the thermal stresses (radial, azimuthal and axial stresses), which appear during the cooling of the system (nanowire and alumina template) from room temperature to 3 K was evaluated. The analysis of thermal induced stresses provides useful informations concerning the magnetic anisotropy in the Co nanowires. The temperature dependence of the remanent magnetization and coercitive field as an effect of the induced thermal …


Microwave Absorption Of Patterned Arrays Of Nanosized Magnetic Stripes With Different Aspect Ratios, Leszek M. Malkinski, Minghui Yu, Andriy Y. Voyk, Donald J. Scherer Ii, Leonard Spinu, Weillie Zhou, Scott Whittenburg, Zachary Davis, Jin-Seung Jung Jan 2007

Microwave Absorption Of Patterned Arrays Of Nanosized Magnetic Stripes With Different Aspect Ratios, Leszek M. Malkinski, Minghui Yu, Andriy Y. Voyk, Donald J. Scherer Ii, Leonard Spinu, Weillie Zhou, Scott Whittenburg, Zachary Davis, Jin-Seung Jung

Physics Faculty Publications

Arrays consisting of nanosized stripes of Permalloy with different length-to-width ratios have been fabricated using electron beam nanolithography, magnetron sputtering, and lift-off process. These stripes have a thickness of 100 nm, a width of 300 nm, and different lengths ranging from 300 nm to 100 μm. The stripes are separated by a distance of 1 μm. Magnetization hysteresis loops were measured using a superconducting quantum interference device susceptometer. Microwave absorption at 9.8 GHz was determined by means of ferromagnetic resonance technique. The dependence of the resonant field on the angle between the nanostructure and the in-plane dc magnetic …