Silicon alloys

Articles 1 - 2 of 2

Full-Text Articles in Physics

Variation Of Magnetostriction With Temperature In Tb5si2.2ge1.8 Single Crystal, A. P. Ring, H. L. Ziegler, Thomas A. Lograsso, Deborah L. Schlagel, J. E. Snyder, David C. Jiles Apr 2006

Variation Of Magnetostriction With Temperature In Tb5si2.2ge1.8 Single Crystal, A. P. Ring, H. L. Ziegler, Thomas A. Lograsso, Deborah L. Schlagel, J. E. Snyder, David C. Jiles

Ames Laboratory Conference Papers, Posters, and Presentations

The Tb5(SixGe4−x) alloy system is similar to the better known Gd5(SixGe4−x), except it has a more complex magnetic and structural phase diagram. Gd5(SixGe1−x)4 has received much attention recently due to its giant magnetocaloric effect, colossal magnetostriction and giant magnetoresistance in the vicinity of a first order combined magnetic-structural phase transition. The magnetostriction changes that accompany the phase transitions of single crystal Tb5(Si2.2Ge1.8) have been investigated at temperatures between 20 and150 K by measurements of ...


Spontaneous Generation Of Voltage In Single-Crystal Gd5si2ge2 During Magnetostructural Phase Transformations, Min Zou, H. Tang, Deborah L. Schlagel, Thomas A. Lograsso, Karl A. Gschneidner Jr., Vitalij K. Pecharsky Apr 2006

Spontaneous Generation Of Voltage In Single-Crystal Gd5si2ge2 During Magnetostructural Phase Transformations, Min Zou, H. Tang, Deborah L. Schlagel, Thomas A. Lograsso, Karl A. Gschneidner Jr., Vitalij K. Pecharsky

Ames Laboratory Conference Papers, Posters, and Presentations

The spontaneous generation of voltage (SGV) in single-crystal and polycrystallineGd5Si2Ge2 during the coupled magnetostructural transformation has been examined. Our experiments show reversible, measurable, and repeatable SGV responses of the materials to the temperature and magnetic field. The parameters of the response and the magnitude of the signal are anisotropic and rate dependent. The magnitude of the SGV signal and the critical temperatures and critical magnetic fields at which the SGV occurs vary with the rate of temperature and magnetic-field changes.